General datasheets for 34 injection molding resins. Processing, drying, temperature and mold geometry ranges.

The ranges shown in these data tables were compiled by the MVPS team from various parameter sheets and literature, integrating the lower and upper limits for each material type.

This information must be carefully reviewed when developing injection molding processes. Final ranges and processing tolerances are the responsibility of the engineer in charge.

These ranges are not recommended for developing specific process tolerances. MVPS always recommends requesting and consulting the supplier's data sheet.

ABS

ABS

Acrilonitrilo Butadieno Estireno

Melt
241–271°C
Shrinkage
0.7–1.6%
PolystyrenesView
PP

PP

Polipropileno

Melt
220–279°C
Shrinkage
1–3%
PolyolefinsView
PC

PC

Policarbonato

Melt
277–338°C
Shrinkage
0.5–0.7%
PolycarbonatesView
PA6

PA6

Poliamida 6 (Nylon)

Melt
232–288°C
Shrinkage
0.5–1.5%
PolyamidesView
HDPE

HDPE

Polietileno de Alta Densidad

Melt
179–282°C
Shrinkage
1.5–4%
PolyethylenesView
POM

POM

Polioximetileno (Acetal)

Melt
193–216°C
Shrinkage
1.5–2.5%
EngineeringView
PMMA

PMMA

Polimetil Metacrilato (Acrílico)

Melt
218–279°C
Shrinkage
0.2–0.8%
AcrylicsView
LDPE

LDPE

Polietileno de Baja Densidad

Melt
179–191°C
Shrinkage
2–5%
PolyethylenesView
PS

PS

Poliestireno

Melt
166–229°C
Shrinkage
0.1–0.7%
PolystyrenesView
PBT

PBT

Tereftalato de Polibutileno

Melt
229–271°C
Shrinkage
0.5–2%
PolyestersView
PA66

PA66

Poliamida 66 (Nylon)

Melt
279–299°C
Shrinkage
0.8–3%
PolyamidesView
PA12

PA12

Poliamida 12 (Nylon)

Melt
241–260°C
Shrinkage
0.7–2%
PolyamidesView
PA12-

PA12-GF

Poliamida 12 + Fibra de Vidrio

Melt
227–238°C
Shrinkage
0.7–2%
PolyamidesView
ASA

ASA

Acrilonitrilo Estireno Acrilato-Nitrilo

Melt
202–229°C
Shrinkage
0.4–0.7%
PolystyrenesView
GPPS

GPPS

Poliestireno de Uso General

Melt
191–221°C
Shrinkage
0.4–0.7%
PolystyrenesView
HIPS

HIPS

Poliestireno de Alto Impacto

Melt
218–246°C
Shrinkage
0.2–0.8%
PolystyrenesView
PET

PET

Tereftalato de Polietileno

Melt
282–299°C
Shrinkage
0.3–3%
PolyestersView
CAP

CAP

Propionato de Acetato de Celulosa

Melt
185–196°C
Shrinkage
0.3–1%
CellulosicsView
CPVC

CPVC

Cloruro de Polivinilo Clorado

Melt
204–216°C
Shrinkage
0.3–0.7%
PVCView
FPVC

FPVC

Cloruro de Polivinilo (Flexible)

Melt
160–193°C
Shrinkage
0.2–0.6%
PVCView
PVC

PVC

Cloruro de Polivinilo (Rígido)

Melt
185–204°C
Shrinkage
0.1–0.6%
PVCView
PE

PE

Polietileno

Melt
254–277°C
Shrinkage
0.2–0.8%
PolyethylenesView
PPE

PPE

Éter de Polifenileno

Melt
260–310°C
Shrinkage
0.5–0.8%
PolyolefinsView
LCP

LCP

Polímero de Cristal Líquido

Melt
279–343°C
Shrinkage
0.1–0.6%
High PerformanceView
PEEK

PEEK

Poliéter Éter Cetona

Melt
354–377°C
Shrinkage
1.2–1.6%
High PerformanceView
PEI

PEI

Polieterimida (Ultem)

Melt
338–416°C
Shrinkage
0.6–0.8%
High PerformanceView
PES

PES

Polietersulfona (PESU)

Melt
288–410°C
Shrinkage
0.5–0.7%
High PerformanceView
PPS

PPS

Polisulfuro de Fenileno

Melt
307–341°C
Shrinkage
0.6–1.4%
High PerformanceView
PPSU

PPSU

Polifenilsulfona

Melt
343–377°C
Shrinkage
0.7–0.9%
High PerformanceView
TPA

TPA

Poliamida Termoplástica Elastómera

Melt
152–199°C
Shrinkage
0.3–1.4%
Thermoplastic ElastomersView
TPE

TPE

Elastómero Termoplástico

Melt
221–241°C
Shrinkage
1–2%
Thermoplastic ElastomersView
TPO

TPO

Poliolefina Termoplástica

Melt
204–232°C
Shrinkage
0.8–1%
Thermoplastic ElastomersView
TPU

TPU

Poliuretano Termoplástico

Melt
216–229°C
Shrinkage
0.1–1.2%
Thermoplastic ElastomersView
TPV

TPV

Termoplástico Vulcanizado

Melt
193–232°C
Shrinkage
1.4–2.5%
Thermoplastic ElastomersView